316L Stainless Steel Plate can be welded by manual argon arc welding (MTIG) or CO2 welding method or by manual welding.

Manual argon arc welding: ER316L welding wire, 2.5 thick or 3.2 thick can be used; for 6mm thick plate can use X-shaped groove, welding welding should pay attention to the welding deformation problem, can be a front side, the opposite side, try to offset the welding deformation zone Impact

CO2 welding method of 316L Stainless Steel Coil: If you want to get better results, you can use the flux-cored wire (E316LT) for tailor welding. The reason for selecting the core is that the splash is very small, the weld protection effect is good, but the price is more expensive. Pay attention to the operation of clearing the roots during operation, and then remove the coating before performing the next welding. Manual electrode welding: It can also be processed by manual electrode welding. Select A207 electrode for welding. Welding of the electrodes also requires the operation of layer cleaning.

316L Stainless Steel Plate

Sign up to receive our newsletter and exclusive discounts and offters.

  • +86 22 8688 9302
  • info@detect-metals.com
  • 2404, Red Star International Building, Jingjin Road, Beichen District, Tianjin, China 300400
Copyright © 310s Stainless Steel Plate, 316l Stainless Steel Plate, 416 Stainless Steel Bar Supplier All Rights Reserved     Powered by
Skype
Whatsapp
E-mail